Shenzhen Alu Rapid Prototype Precision Co., Ltd.
Industry News
- Home
- News
- Aluminium Prototyping and CNC Machining: Grades, Tolerances and Finishes
Aluminium Prototyping and CNC Machining: Grades, Tolerances and Finishes
British and European buyers search for aluminium; American buyers search for aluminum. Google treats them as different queries, and a site that only ever writes the American spelling never appears for roughly a third of the English-speaking market.
This guide covers prototyping and machining in aluminium, with the specifications European buyers actually ask for: EN AW grades, metric tolerances, and surface finishes to ISO and Qualanod standards.
Aluminium grades, in both naming systems
| EN / ISO designation | US designation (AA) | Machinability | Typical use |
|---|---|---|---|
| EN AW-6082 | 6061 | Good | General machining, structural parts, enclosures |
| EN AW-7075 | 7075 | Fair | High-strength parts, moulds, aerospace |
| EN AW-5754 | 5052 | Poor (sheet) | Sheet metal enclosures, marine |
| EN AW-5083 | 5083 | Poor | Marine, welded structures |
| EN AW-2011 | 2011 | Excellent | Screw-machined precision parts |
| EN AW-1050 / 1100 | 1050 / 1100 | Fair | Forming, heat sinks, electrical |
The practical upshot: 6082-T6 and 6061-T6 are the same family and behave almost identically. If your drawing says 6082 and the shop quotes 6061, the difference is negligible for most parts — but confirm it in writing, because a certification mismatch can fail an incoming inspection.
Prototyping processes for aluminium
CNC machining (subtractive)
The default for functional aluminium prototypes. Tolerance ±0.05 mm standard, ±0.01 mm where specified. Lead time 3–7 working days. See CNC machining services.
Sheet metal fabrication
For enclosures and brackets in 1–3 mm sheet. No tooling cost, so prototype and production economics are nearly identical at low volume. See sheet metal fabrication and our guide to bend reliefs.
Die casting
For quantities above roughly 1,000 units. Aluminium die casting uses A380/ADC12 in US and Asian practice, or EN AC-46000 in European practice. Tooling cost means it is rarely a prototype process, though prototype tooling is available.
Vacuum casting (for comparison parts)
Not for aluminium itself — but polyurethane castings that mimic anodised aluminium appearance are a standard way to validate a design before committing to metal.
Finishes: the European specification
| Finish | Standard | Notes |
|---|---|---|
| Clear anodising | ISO 7599, Qualanod | 10–25 µm typical; colour varies by alloy |
| Hard anodising | ISO 10074 | 25–50 µm; wear surfaces, Type III |
| Chromate conversion | MIL-DTL-5541 / ISO 8079 | Conductive, corrosion protection, paint base |
| Powder coating | ISO 15184 | RAL colours; 60–80 µm per surface |
| Bead blasting | — | Ra 1.6–3.2 µm uniform matte; often before anodising |
Two European requirements that catch US-oriented suppliers out: RoHS and REACH declarations for the alloy and the coating, and material certificates to EN 10204 3.1 rather than a generic mill certificate.
Tolerances in metric
| Feature | Standard | Precision |
|---|---|---|
| Linear dimension | ±0.1 mm | ±0.02 mm |
| Hole diameter | H12 | H7 |
| Flatness, 100 mm | 0.05 mm | 0.02 mm |
| Perpendicularity | 0.1 mm | 0.03 mm |
| Surface roughness | Ra 1.6–3.2 µm | Ra 0.4 µm |
ISO 2768-m is the usual general tolerance callout on European drawings. If your drawing uses it, say so — a shop quoting to a tighter internal standard will price higher than necessary.
What drives the price of an aluminium prototype
Setup count. Features on five faces means five setups. This dominates at quantity one.
Material removal. A part machined from a solid billet pays for every cubic centimetre of air.
Wall thickness. Below 1 mm, chatter and distortion require slower feeds and more scrap.
Tolerance. Tight tolerance on every feature rather than the critical three can double the price.
Finishing. Anodising adds 2–5 days and a batch minimum; multiple colours multiply the cost.
Frequently asked questions
Is aluminium or aluminum correct?
Both. "Aluminium" is the IUPAC and British/European form; "aluminum" is the American form. The metal is identical.
What is the best aluminium for prototyping?
6082/6061-T6 for almost everything: good machinability, weldability, corrosion resistance and anodising response.
How fast can I get an aluminium prototype?
Three to seven working days for CNC machining at quantity one, plus transit. Add three to five days if anodising is required.
Can aluminium prototypes be welded?
Yes, 6082 and 5754 weld well. 7075 and 2024 are generally not weldable and should be mechanically fastened or bonded.
Do I need a material certificate?
For regulated or export work, yes — ask for EN 10204 3.1 with the heat number traceable to the parts.
Next step
Send a STEP file with the alloy, the general tolerance standard your drawing uses, and the finish specification. A supplier familiar with European work will confirm the EN grade and the certificate type before quoting.
References
Aluprototype machines and finishes aluminium prototypes in Shenzhen to ISO 2768 and ISO 7599, with EN 10204 3.1 certificates on request. ISO 9001:2015 certified. Request an aluminium prototyping quote →