Shenzhen Alu Rapid Prototype Precision Co., Ltd.
Industry News
- Home
- News
- Hollow Parts for SLS and MJF: Drain Holes and Powder Removal
Hollowing an SLS or MJF part can reduce fused material, lower weight, improve thermal uniformity, and sometimes reduce cost. However, a hollow CAD model is not automatically an empty finished part. Selective laser sintering (SLS) and Multi Jet Fusion (MJF) build parts inside a bed of powder, so every enclosed cavity fills with unfused material during production. That powder stays trapped unless the geometry provides practical access for removal.
A successful hollow design therefore needs more than a shell command in CAD. The designer must choose a suitable wall thickness, connect every internal chamber to the outside, size and locate drain holes for real cleaning tools, avoid blind pockets, and define how the supplier will verify that the required powder has been removed. This guide explains how to design hollow SLS and MJF nylon parts that can be printed, depowdered, inspected, and used reliably.
Quick Answer: How Should You Design a Hollow SLS or MJF Part?
Use the following starting checklist, then confirm the final values with the selected material and printing supplier:
Create a consistent shell instead of abrupt transitions between very thick and very thin sections.
Give every enclosed cavity at least two openings so powder can leave while air enters.
Place openings on different sides of the cavity, preferably with a clear cleaning path.
Make holes large enough for the supplier's vacuum, air, brush, or blasting process.
Avoid long blind passages, sharp internal corners, narrow necks, and isolated chambers.
Keep lattice openings large enough for powder to move through the structure.
Decide whether drain holes may remain open, be plugged, or be hidden by assembly.
Specify a cleaning and verification requirement when residual powder affects mass, balance, airflow, hygiene, or performance.
Published guidelines vary by machine, material, and provider. Formlabs recommends at least two drain holes of 3.5 mm or larger for its Fuse-series SLS cavities. The HP MJF handbook published with Protolabs recommends two holes on opposite faces and a 5 mm minimum diameter for efficient powder removal. Treat these figures as process-specific starting points, not universal guarantees.
Why Hollow Powder-Bed Parts Need Special Design Rules
SLS uses a laser to fuse selected regions of polymer powder. MJF applies functional agents and heat to fuse the required areas. In both processes, unfused powder surrounds and supports the part during the build. This support enables complex shapes, undercuts, internal passages, and nested assemblies without the attached support structures common in many other 3D printing methods.
The same powder that supports the geometry also occupies every internal void. After cooling, the supplier removes the build from the powder cake and cleans exposed surfaces. Powder inside a sealed cavity cannot escape. Powder inside a poorly accessible cavity may move slightly but remain packed in corners, channels, and lattice cells.
Trapped powder may create several problems:
The finished part weighs more than the CAD mass predicts.
Loose powder can leak later through a small opening.
Residual material can block airflow, acoustic paths, or cable routes.
Moving powder can change balance or create noise.
Internal contamination may be unacceptable for a clean product.
A customer may pay for hollow geometry without receiving the expected weight reduction.
A cavity may be intentionally left full when weight is not critical and cleaning access would compromise the design. That can save post-processing effort, but it must be a conscious decision. The drawing, CAD notes, and supplier quotation should state whether the cavity is intended to be empty, partly cleaned, or permanently powder-filled.
When Should You Hollow an SLS or MJF Part?
Good reasons to hollow
Reducing the mass of a large housing, model, duct, or ergonomic prototype.
Avoiding excessive heat accumulation in a thick cross-section.
Reducing fused material volume where the supplier's pricing model rewards it.
Creating room for wiring, electronics, insulation, or later assembly.
Moving the center of mass or meeting a weight target.
Reasons to keep a part solid
The part is small and the weight saving is negligible.
The shell would reduce strength, stiffness, impact resistance, or thread engagement.
Drain openings are not acceptable on cosmetic or sealed surfaces.
The internal shape cannot be cleaned or verified.
The hollowing work and cleaning cost exceed the material saving.
The part must be pressure-tight and sealing the access holes would create more risk.
Do not assume that a hollow part is always cheaper. Some suppliers price mainly by bounding volume, build packing, machine time, and post-processing rather than by fused mass alone. A hollow model can also require more manual depowdering. Ask the supplier to compare a solid version, a hollow version, and—when appropriate—a ribbed or lattice-reinforced version.
Shell Thickness: Balance Weight, Printability, and Strength
The minimum printable wall is not automatically the correct structural wall. A thin coupon may print successfully but a large hollow housing with the same wall can warp, dent during blasting, or crack around a drain hole. Wall capability depends on material, wall span, curvature, orientation, thermal history, finishing, and service load.
For initial DFM, consider:
Local span: large flat shells usually need more thickness or ribs than small curved shells.
Material: PA12, glass-filled nylon, and TPU have different stiffness and cleaning behavior.
Openings: drain holes reduce local load area and can create stress concentrations.
Fasteners: bosses, inserts, and threads require enough surrounding material.
Finishing: blasting, tumbling, sanding, and dyeing may damage delicate walls or remove material.
Use condition: pressure, impact, heat, creep, moisture, and repeated handling may control the design.
Use gradual transitions between a shell, ribs, bosses, and thick mounting features. Sharp thickness changes can concentrate stress and create uneven thermal behavior. Add generous internal fillets where ribs or bosses meet the shell. If a boss must remain solid, blend it into the wall rather than placing a heavy isolated mass on a thin panel.
Drain Holes and Escape Holes: The Core Design Feature
The terms drain hole, escape hole, and powder-removal hole are often used interchangeably. For powder-bed polymer printing, their purpose is to provide physical access for unfused powder to leave the cavity and for cleaning air or tools to enter.
Use at least two openings per cavity
One hole can allow some powder to fall out, but cleaning becomes inefficient because air cannot circulate freely. Two separated openings provide an inlet and outlet. They also let the operator change the cleaning direction and break powder bridges.
Every isolated chamber needs its own route. A part with three cavities connected only in the designer's imagination is still three sealed powder traps. Review the final Boolean geometry and sectional views to confirm that each chamber communicates with the outside.
Locate openings on different sides
Opposed or well-separated openings are usually easier to clean than adjacent holes. A clear line of sight is valuable because the operator can direct compressed air, a vacuum nozzle, or a probe through the cavity. Put at least one hole near a natural low point for gravity-assisted emptying, but remember that the part will be rotated repeatedly during cleaning.
Good locations include:
Surfaces hidden by a cover, label, plug, or mating component.
Ends of a long internal volume.
Areas that can be reached without damaging cosmetic faces.
Regions with sufficient wall thickness and edge distance.
Avoid placing a small hole at the end of a deep funnel-shaped pocket. Powder compacts around sharp internal corners and may not flow toward the opening. A short cylindrical port with a smooth internal transition is easier to clean and easier to plug later.
Make holes large enough for the real process
A hole can be printable but too small for dependable depowdering. The required diameter depends on powder particle behavior, cavity volume, passage length, wall thickness, material, and cleaning equipment. Small holes are also more likely to shrink, partially fuse, or become blocked by adhered powder.
As practical reference points, Formlabs specifies two 3.5 mm or larger drain holes for many Fuse SLS cavities, while the HP MJF handbook recommends two 5 mm holes on opposite faces. Larger holes and more direct access generally make cleaning faster and more complete. Confirm the provider's own minimum before releasing the file.
For a large cavity, simply meeting a minimum diameter may be inadequate. Ask whether the cleaning operator can insert the intended nozzle and whether the volume can be inspected. If the hole will be threaded, reamed, or plugged, leave enough stock and edge distance for the secondary operation.
Internal Channels: Diameter Alone Is Not Enough
A short straight bore can be depowdered more easily than a long curved channel of the same diameter. Cleaning difficulty increases with length, bends, changes in cross-section, rough internal surfaces, branches, and blind ends.
For internal passages:
Prefer straight or gently curved routes with access at both ends.
Avoid sudden contractions that create a powder choke point.
Use large bend radii rather than sharp elbows.
Give each branch a cleaning path.
Add removable cleanout plugs when a long path cannot be reached from the main ports.
Increase the passage size as length and complexity increase.
Do not rely on compressed air alone for a critical fluid channel.
If the passage carries air, coolant, vacuum, or liquid, define an acceptance test. Depending on the application, this may be a flow test, pressure-drop check, borescope inspection, mass check, CT scan, or cleanliness test. A nominally open channel is not proof that the required cross-section is clean along its full length.
Lattice Structures and Powder Removal
Lattices can reduce fused mass and tune stiffness, cushioning, energy absorption, or airflow. They also create many small cells and contact points that hold powder. A visually open lattice in CAD may be difficult to clean when it is enclosed by a shell.
The HP MJF design-for-cleaning guidance recommends a minimum 5 mm lattice gap when powder must be removed and notes that a partially open lattice is easier to clean. The correct gap still depends on lattice depth, cell topology, material, and access direction.
Before choosing an enclosed lattice, decide which of these outcomes is acceptable:
Powder fully removed: provide broad access and an inspectable structure.
Powder partly removed: accept a mass range and possible residual movement.
Powder intentionally trapped: seal the structure and account for the retained mass.
An internal lattice can make the part heavier than expected if powder remains. It can also behave inconsistently if one batch is cleaned more thoroughly than another. For repeat production, specify a mass window or other measurable cleanliness criterion rather than an ambiguous instruction such as “remove all powder.”
Designing Drain Holes That Can Be Closed Later
Many products cannot keep visible holes. Plan the closure method during CAD design instead of asking the finishing team to improvise after printing.
Common closure options
Press-fit printed plugs with adhesive.
Threaded plugs in machined or tapped ports.
Heat-staked or bonded plastic caps.
A label, trim piece, gasket, or assembly cover over the opening.
Welding or controlled thermal sealing for compatible materials.
Leaving the hole open where ventilation is acceptable.
A plug is not automatically leak-tight. If the hollow part must resist water, dust, pressure, vacuum, chemicals, or repeated temperature cycles, define the seal geometry and test method. A threaded plug may need a gasket or sealant. An adhesive joint needs enough bond area, suitable surface preparation, and compatibility with nylon and any dye or coating.
Keep plug ports away from high-stress regions. Add a flat seating face when a gasket is used, and allow machining stock if the as-printed surface is too rough for sealing.
Depowdering and Post-Processing Workflow
Design quality and cleaning quality are linked. A typical workflow may include:
Allowing the build to cool according to the validated process.
Removing the part from the powder cake.
Brushing and vacuuming loose exterior powder.
Rotating, tapping, vacuuming, and blowing through drain holes.
Media blasting accessible surfaces.
Repeating cleaning from multiple directions.
Inspecting or weighing the part.
Applying dye, tumble finishing, coating, sealing, or machining.
Compressed air must be used with appropriate extraction and personal protective equipment. Powder can become airborne, and uncontrolled high pressure may drive material deeper into a pocket or damage a thin feature. Cleaning procedures should follow the printer and material supplier's safety guidance.
Post-processing can change the hole and shell. Tumbling may round an opening, blasting may erode a delicate edge, and dye can reveal inconsistent cleaning. If a hole is later reamed or tapped, sequence the operations so new chips do not become trapped in the cavity.
How to Verify Powder Removal
The right verification method depends on the consequence of residual powder. A visual check may be enough for a concept model. A medical fixture, airflow manifold, balanced rotor, or sealed electronics enclosure may require objective evidence.
Practical verification methods
Mass comparison: compare the cleaned part with the expected mass and an approved reference sample.
Shake and sound test: useful for detecting loose powder, but not compacted material.
Borescope inspection: effective when ports provide line-of-sight access.
Airflow or pressure-drop test: suitable for functional channels.
CT scanning: valuable for critical internal structures, though cost and resolution must be considered.
Sectioned first article: destructive validation can confirm a new cleaning process before production release.
Cleanliness collection: flush or agitate under a controlled method and measure extracted residue when the application permits.
Mass inspection works only when moisture conditioning, material variation, dye, plugs, and dimensional tolerances are controlled. Nylon absorbs moisture, so state the conditioning method and weighing time if the mass limit is tight.
Common Hollow-Part Design Mistakes
One tiny hole for a large cavity
The opening may technically connect the cavity to the outside but cannot support efficient cleaning. Add a second opening and increase access.
Multiple chambers with only one connected
Thin ribs or internal walls can divide a shell into sealed zones. Use section analysis and flow-path review to confirm connectivity.
A long internal channel with a blind end
Powder compacts at the end and cannot be driven through. Open both ends or add a cleanout port.
Drain holes added after design release
Late holes often interfere with cosmetic surfaces, fasteners, sealing, or assembly. Include them in the functional CAD model and drawing.
Using the process minimum as the production target
A minimum printable hole may not be a cleanable hole. Design for a stable post-processing window, not a borderline feature.
Ignoring retained powder in weight calculations
If powder remains, the measured mass will exceed the shell's CAD mass. Define whether the weight target assumes an empty or filled cavity.
No acceptance criterion
“Clean inside” can mean different things to different people. Specify mass, flow, visual access, residue, or an approved sample.
DFM Checklist for Hollow SLS and MJF Parts
Is hollowing necessary for weight, thermal behavior, function, or cost?
Is the shell thick enough for its span, material, finish, and load?
Are wall transitions gradual and filleted?
Does every cavity connect to the exterior?
Are there at least two useful openings per cavity?
Do opening size and location match the supplier's cleaning equipment?
Can long channels be accessed from both ends?
Can powder pass through every lattice cell and branch?
Will plugs, labels, or covers close the openings after cleaning?
Are sealing, pressure, airflow, and cleanliness tests defined?
Are mass targets based on a stated moisture and cleaning condition?
Has the supplier approved the design for the exact machine and material?
What to Send With an RFQ
To receive an accurate quotation and useful DFM feedback, send:
A STEP file plus the printable STL or 3MF file when available.
The selected process: SLS or MJF.
Material and color requirements.
Quantity, batch size, and expected repeat orders.
Critical dimensions and tolerances.
Target part mass or maximum allowable retained powder.
A section view showing all internal chambers and channels.
Drain-hole locations, minimum diameters, and closure method.
Required surface finish, dye, coating, or machining.
Airflow, pressure, leak, balance, or cleanliness tests.
Whether the supplier may modify drain holes or shell thickness with approval.
Ask the supplier to identify any cavity that cannot be cleaned or inspected. Also request confirmation of the planned build orientation, cleaning method, and any geometry changes before production.
Frequently Asked Questions
Do hollow SLS and MJF parts always need drain holes?
They need openings if the unfused powder must be removed. A completely sealed cavity can be printed, but it will retain powder. State this intention explicitly and include the retained mass in the design.
How many drain holes should a hollow part have?
Use at least two effective openings for each powder-trapping cavity. Complex, large, divided, or long cavities may need more. The goal is a complete air and powder flow path, not merely a hole count.
What drain-hole diameter should I use?
Follow the selected supplier's rule for the exact machine and material. Published examples include two 3.5 mm or larger openings for Formlabs Fuse SLS cavities and two 5 mm openings for the HP MJF cleaning guidance. Larger or deeper cavities often need larger access.
Can compressed air remove all powder from an internal channel?
Not necessarily. Powder may bridge, compact in corners, or adhere to rough internal surfaces. Use access from both ends and verify critical passages with flow, mass, borescope, CT, or another suitable method.
Is a hollow printed part as strong as a solid part?
Usually not under every load case. Strength and stiffness depend on shell thickness, shape, ribs, openings, material, orientation, and loading. Analyze or test the hollow configuration rather than applying solid-part data directly.
Can drain holes be hidden?
Yes. Put them under a cover, label, plug, or mating component when practical. Their location must still allow effective cleaning before closure.
Does hollowing always reduce price?
No. It reduces fused material, but pricing may also depend on bounding volume, packing, build time, machine utilization, and manual cleaning. Request a direct quotation comparison.
Conclusion
Hollow SLS and MJF parts succeed when the CAD model is designed for both printing and cleaning. Use a structurally appropriate shell, connect every cavity to the outside, provide multiple generous drain holes, simplify internal channels, and make lattice regions accessible. Then define how powder removal will be verified and how openings will be closed.
Aluprototype provides SLS and MJF 3D printing for functional prototypes and low-volume production parts. Send your 3D model, material, quantity, internal-cleanliness requirement, critical dimensions, and finishing needs for DFM feedback and a quotation.