Shenzhen Alu Rapid Prototype Precision Co., Ltd.

Industry News

  • Home
  • News
  • Powder Removal in SLS and MJF 3D Printing: How to Design and Verify Internal Channels

Powder Removal in SLS and MJF 3D Printing: How to Design and Verify Internal Channels

A 3D-printed nylon duct can have clear openings and still hold powder behind an internal turn. In selective laser sintering (SLS) and Multi Jet Fusion (MJF), the surrounding powder supports the part during printing. After the build, unfused powder must be removed from any cavity or passage where it could restrict flow, shed particles or change the part’s mass. Plan the route for removing it and the method for checking that route before releasing the CAD.

Design a path for powder to leave

Start with a section view. Follow each passage from its opening to its narrowest point, then look for bends, blind branches and pockets behind ribs. Where the design allows, provide access from both ends so the shop can work through the passage and give dislodged powder an exit. Place cleanout ports near the pockets they serve. A large opening at one end offers limited help if powder must still pass through a narrow throat farther inside.

Use the provider’s design rules for the selected machine and powder. Formlabs, for example, lists two escape holes of at least 3.5 mm for each powder-trapping cavity in its Fuse Nylon 12 specifications. That figure is a starting point for the stated process and geometry. Review long passages, bends and tool access separately. Formlabs Fuse Nylon 12 design specifications

Feature in the CADChange to consider before printing
Long through-channel with a sharp turnAdd access near the turn, increase the bend radius where space permits, or split the duct into two pieces that can be cleaned before assembly.
Blind branch behind an internal ribOpen the branch to an accessible face or change the rib layout so it leaves a continuous route to an exit.
Hollow shell with a lattice coreTrace a path through the actual cells. Check the smallest opening between cells and where the lattice meets the shell.
Cleanout port that will receive a plugAgree on the cleaning and inspection sequence before plugging. Check that the plug leaves the intended flow area and meets any sealing requirement.

Match the inspection method to the failure you need to detect

Look inside where you have access. Use a light or borescope to inspect reachable walls and junctions. Record which regions the inspection covers. For an initial build, a sectioned sample or representative coupon can expose the bend or branch that the borescope cannot reach. Match the coupon’s passage length, cross-section and build orientation to the feature of concern.

Check function where restriction matters. For a duct or manifold, agree on a flow or pressure-drop check with specified connections and test conditions. If multiple branches share an outlet, test branches separately where practical. A good total flow reading can hide a restriction in one branch. If loose particles are the concern, define a separate particle collection check and an acceptance limit tied to the application.

Validate any indirect check. Stable mass after successive cleaning passes can help monitor the process, but a fixed mass can also mean that residual powder is staying put. For inaccessible passages, ask whether X-ray imaging can resolve the suspected deposit in that material and geometry. Published MJF research used industrial X-ray imaging to assess residual powder in test parts. Validate the method on a representative sample before relying on it for acceptance. Experimental study of accuracy and powder removal limits in MJF

Example with a nylon electronics cooling duct

Consider a duct that turns around a mounting boss and splits into two outlets. Both outlets look open, but the branch behind the boss delivers less airflow. The revised CAD adds a cleanout port beside the turn. The first build includes a spare duct for sectioning so the team can examine the pocket behind the boss and compare what it finds with the branch flow readings.

For later builds, the team inspects through the cleanout port before fitting its plug, then checks the flow at each outlet with the duct assembled. If particle shedding could affect the electronics, the drawing or purchase order also specifies how to collect and assess released particles. These checks address different ways residual powder can affect the part.

What to send with an SLS or MJF quote request

  • Send the CAD model and a section view marking every internal passage that needs cleaning.

  • Identify the narrowest cross-section, blind branches, and the faces where cleanout ports or split lines are allowed.

  • State whether the concern is blocked flow, particle shedding, mass or a combination. Include the inspection method and acceptance criteria if already defined.

  • Ask whether the first build should include a sectionable sample, and whether cleaning and inspection need to happen before plugs or other hardware are installed.

Share the marked CAD and the intended use of the part so cleaning access and inspection can be reviewed with the print geometry. Request a 3D printing quote from Aluprototype.

References